Abstract

The low-carbon and low-cost cement known as limestone–calcined clay cement (LC3) is used in this study to investigate the immobilization potential of Pb-Zn smelter residue (LZSR). The performance of LC3 treatment on LZSR was determined through a series of experiments, including pH, unconfined compressive strength (UCS), toxicity characteristic leaching procedure (TCLP), Community Bureau of Reference sequential extraction procedure (BCR-SEP), Fourier-transform infrared spectroscopy (FTIR), thermogravimetric analysis (TGA), X-ray diffraction (XRD), and scanning electron microscopy along with energy dispersive spectroscopy (SEM-EDS). The findings show that, after 14 days curing, the transition in the pH from acid to alkaline increases the UCS up to 2.5–3.6 times compared with untreated specimens. The leached concentrations of Pb, Zn, and Cd decreased considerably with increasing binder and curing time. Chemical speciation analysis showed that >50% of bioavailable phases (acid-soluble and reducible phases) were transformed into less soluble (oxidizable and residual) phases. The XRD and SEM-EDS analysis demonstrated that the formation of favorably insoluble alite (Ca3SiO5), meionite (Ca4Al6Si6O24CO3), and portlandite (Ca(OH)2) was responsible for the immobilization of Pb, Zn, and Cd. As a result, LC3 supports the green and sustainable remediation approach for the immobilization of heavy metals for the potential valorization of LZSR.

Get full access to this article

View all available purchase options and get full access to this article.

Acknowledgments

The authors thank Hindustan Zinc Limited (HZL), Rajasthan, India, for providing the Pb-Zn smelter residue (LZSR), Technological Action and Rural Advancement (TARA), Delhi, India, for providing the LC3 binder, and the Applied Chemistry Department (ACD) at Sardar Vallabhbhai National Institute of Technology, Surat, India, for help with the spectroscopy and thermal analysis.

References

Antoni, M., J. Rossen, F. Martirena, and K. Scrivener. 2012. “Cement substitution by a combination of metakaolin and limestone.” Cem. Concr. Res. 42 (12): 1579–1589. https://doi.org/10.1016/j.cemconres.2012.09.006.
ASTM. 2001. Standard test method for pH of soils. ASTM D4972, West Conshohocken, PA: ASTM.
ASTM. 2002. Standard test method for specific gravity of soil solids by water pycnometer. ASTM D 854, West Conshohocken, PA: ASTM.
ASTM. 2007. Standard test methods for moisture, ash, and organic matter of peat and organic soils. ASTM D2974. West Conshohocken, PA: ASTM.
ASTM. 2008. Standard test method for unconfined compressive strength index of chemical-grouted soils. ASTM D4219, West Conshohocken, PA: ASTM.
ASTM. 2010a. Standard test methods for laboratory determination of water (moisture) content of soil and rock by mass. ASTM D2216, West Conshohocken, PA: ASTM.
ASTM. 2010b. Standard test methods for liquid limit, plastic limit, and plasticity index of soils. ASTM D4318. West Conshohocken, PA: ASTM.
ASTM. 2011. Standard practice for classification of soils for engineering purposes (Unified Soil Classification System). ASTM D2487, West Conshohocken. PA: ASTM.
Buanuam, J., J. Shiowatana, and P. Pongsakul. 2005. “Fractionation and elemental association of Zn, Cd and Pb in soils contaminated by Zn minings using a continuous-flow sequential extraction.” J. Environ. Monit. 7 (8): 778–784. https://doi.org/10.1039/b500834d.
Catalan, L. J. J., E. Merlieère, and C. Chezick. 2002. “Study of the physical and chemical mechanisms influencing the long-term environmental stability of natrojarosite waste treated by stabilization/solidification.” J. Hazard. Mater. 94 (1): 63–88. https://doi.org/10.1016/S0304-3894(02)00059-6.
Chiu, A. C. F., R. Akesseh, I. M. Moumouni, and Y. Xiao. 2019. “Laboratory assessment of rice husk ash (RHA) in the solidification/stabilization of heavy metal contaminated slurry.” J. Hazard. Mater. 371: 62–71. https://doi.org/10.1016/j.jhazmat.2019.02.051.
Coudert, E., M. Paris, D. Deneele, G. Russo, and A. Tarantino. 2019. “Use of alkali activated high-calcium fly ash binder for kaolin clay soil stabilisation: Physicochemical evolution.” Constr. Build. Mater. 201: 539–552. https://doi.org/10.1016/j.conbuildmat.2018.12.188.
Dai, Z., et al. 2018. “Speciation analysis and leaching behaviors of selected trace elements in spent SCR catalyst.” Chemosphere 207: 440–448. https://doi.org/10.1016/j.chemosphere.2018.05.119.
da Silva Andrade, D., J. H. da Silva Rêgo, P. C. Morais, A. N. de Mendonça Lopes, and M. F. Rojas. 2019. “Investigation of C-S-H in ternary cement pastes containing nanosilica and highly-reactive supplementary cementitious materials (SCMs): Microstructure and strength.” Constr. Build. Mater. 198: 445–455. https://doi.org/10.1016/j.conbuildmat.2018.10.235.
Davidson, C. M., A. L. Duncan, D. Littlejohn, A. M. Ure, and L. M. Garden. 1998. “A critical evaluation of the three-stage BCR sequential extraction procedure to assess the potential mobility and toxicity of heavy metals in industrially-contaminated land.” Anal. Chim. Acta 363 (1): 45–55. https://doi.org/10.1016/S0003-2670(98)00057-9.
de Andrade Lima, L. R. P., and L. A. Bernardez. 2011. “Characterization of the lead smelter slag in Santo Amaro, Bahia, Brazil.” J. Hazard. Mater. 189 (3): 692–699. https://doi.org/10.1016/j.jhazmat.2011.02.091.
Deboucha, W., N. Leklou, A. Khelidj, and M. N. Oudjit. 2017. “Hydration development of mineral additives blended cement using thermogravimetric analysis (TGA): Methodology of calculating the degree of hydration.” Constr. Build. Mater. 146: 687–701. https://doi.org/10.1016/j.conbuildmat.2017.04.132.
Dhandapani, Y., and M. Santhanam. 2017. “Assessment of pore structure evolution in the limestone calcined clay cementitious system and its implications for performance.” Cem. Concr. Compos. 84: 36–47. https://doi.org/10.1016/j.cemconcomp.2017.08.012.
Du, Y. J., M. L. Wei, K. R. Reddy, and H. L. Wu. 2016. “Effect of carbonation on leachability, strength and microstructural characteristics of KMP binder stabilized Zn and Pb contaminated soils.” Chemosphere 144: 1033–1042. https://doi.org/10.1016/j.chemosphere.2015.09.082.
Feng, Y. S., Y. J. Du, K. R. Reddy, and W. Y. Xia. 2018. “Performance of two novel binders to stabilize field soil with zinc and chloride: Mechanical properties, leachability and mechanisms assessment.” Constr. Build. Mater. 189: 1191–1199. https://doi.org/10.1016/j.conbuildmat.2018.09.072.
Goodarzi, A. R., and M. Movahedrad. 2017. “Stabilization/solidification of zinc-contaminated kaolin clay using ground granulated blast-furnace slag and different types of activators.” Appl. Geochem. 81: 155–165. https://doi.org/10.1016/j.apgeochem.2017.04.014.
Guo, B., B. Liu, J. Yang, and S. Zhang. 2017. “The mechanisms of heavy metal immobilization by cementitious material treatments and thermal treatments: A review.” J. Environ. Manage. 193: 410–422. https://doi.org/10.1016/j.jenvman.2017.02.026.
Hu, H., Q. Deng, C. Li, Y. Xie, Z. Dong, and W. Zhang. 2014. “The recovery of Zn and Pb and the manufacture of lightweight bricks from zinc smelting slag and clay.” J. Hazard. Mater. 271: 220–227. https://doi.org/10.1016/j.jhazmat.2014.01.035.
Kapeluszna, E., Ł. Kotwica, A. Różycka, and Ł. Gołek. 2017. “Incorporation of Al in C-A-S-H gels with various Ca/Si and Al/Si ratio: Microstructural and structural characteristics with DTA/TG, XRD, FTIR and TEM analysis.” Constr. Build. Mater. 155: 643–653. https://doi.org/10.1016/j.conbuildmat.2017.08.091.
Kavitha, O. R., V. M. Shanthi, P. G. Arulraj, and V. R. Sivakumar. 2016. “Microstructural studies on eco-friendly and durable self-compacting concrete blended with metakaolin.” Appl. Clay Sci. 124–125: 143–149. https://doi.org/10.1016/j.clay.2016.02.011.
Krishnan, S., A. C. Emmanuel, V. Shah, A. Parashar, G. Mishra, S. Maity, and S. Bishnoi. 2019. “Industrial production of limestone calcined clay cement: Experience and insights.” Green Mater. 7 (1): 15–27. https://doi.org/10.1680/jgrma.18.00003.
Li, P., C. Lin, H. Cheng, X. Duan, and K. Lei. 2015. “Contamination and health risks of soil heavy metals around a lead/zinc smelter in southwestern China.” Ecotoxicol. Environ. Saf. 113: 391–399. https://doi.org/10.1016/j.ecoenv.2014.12.025.
Li, W., P. Ni, and Y. Yi. 2019. “Comparison of reactive magnesia, quick lime, and ordinary Portland cement for stabilization/solidification of heavy metal-contaminated soils.” Sci. Total Environ. 671: 741–753. https://doi.org/10.1016/j.scitotenv.2019.03.270.
Li, X., and I. Thornton. 2001. “Chemical partitioning of trace and major elements in soils contaminated by mining and smelting activities.” Appl. Geochem. 16 (15): 1693–1706. https://doi.org/10.1016/S0883-2927(01)00065-8.
Li, Y., Y. Chen, C. Tang, S. Yang, J. He, and M. Tang. 2017a. “Co-treatment of waste smelting slags and gypsum wastes via reductive-sulfurizing smelting for valuable metals recovery.” J. Hazard. Mater. 322: 402–412. https://doi.org/10.1016/j.jhazmat.2016.10.028.
Li, Y., Z. Liu, H. Liu, and B. Peng. 2017b. “Clean strengthening reduction of lead and zinc from smelting waste slag by iron oxide.” J. Cleaner Prod. 143: 311–318. https://doi.org/10.1016/j.jclepro.2016.12.108.
Li, Y. C., X. B. Min, L. Y. Chai, M. Q. Shi, C. J. Tang, Q. W. Wang, Y. j. Liang, J. Lei, and W. J. Liyang. 2016. “Co-treatment of gypsum sludge and Pb/Zn smelting slag for the solidification of sludge containing arsenic and heavy metals.” J. Environ. Manage. 181: 756–761. https://doi.org/10.1016/j.jenvman.2016.07.031.
Li, Y. C., X. B. Min, Y. Ke, L. Y. Chai, M. Q. Shi, C. J. Tang, Q. W. Wang, Y. J. Liang, J. Lei, and D. G. Liu. 2018. “Utilization of red mud and Pb/Zn smelter waste for the synthesis of a red mud-based cementitious material.” J. Hazard. Mater. 344: 343–349. https://doi.org/10.1016/j.jhazmat.2017.10.046.
Lothenbach, B., G. Le Saout, E. Gallucci, and K. Scrivener. 2008. “Influence of limestone on the hydration of Portland cements.” Cem. Concr. Res. 38 (6): 848–860. https://doi.org/10.1016/j.cemconres.2008.01.002.
Mao, L., H. Guo, and W. Zhang. 2018. “Addition of waste glass for improving the immobilization of heavy metals during the use of electroplating sludge in the production of clay bricks.” Constr. Build. Mater. 163: 875–879. https://doi.org/10.1016/j.conbuildmat.2017.12.177.
MOEF (Ministry of Environment and Forests). 2016. “Hazardous and other wastes—Ministry of environment and forests.” Gazzate India 1981: 1–68.
Pan, S. Y., K. J. Shah, Y. H. Chen, M. H. Wang, and P. C. Chiang. 2017. “Deployment of accelerated carbonation using alkaline solid wastes for carbon mineralization and utilization toward a circular economy.” ACS Sustainable Chem. Eng. 5 (8): 6429–6437. https://doi.org/10.1021/acssuschemeng.7b00291.
Pan, Y., Z. Wu, J. Zhou, J. Zhao, X. Ruan, J. Liu, and G. Qian. 2013. “Chemical characteristics and risk assessment of typical municipal solid waste incineration (MSWI) fly ash in China.” J. Hazard. Mater. 261: 269–276. https://doi.org/10.1016/j.jhazmat.2013.07.038.
Peña-Icart, M., M. E. Villanueva Tagle, C. Alonso-Hernández, J. R. Hernández, M. Behar, and M. S. Pomares Alfonso. 2011. “Comparative study of digestion methods EPA 3050B (HNO3–H2O2–HCl) and ISO 11466.3 (aqua regia) for Cu, Ni and Pb contamination assessment in marine sediments.” Mar. Environ. Res. 72 (1–2): 60–66. https://doi.org/10.1016/j.marenvres.2011.05.005.
Rauret, G., J. F. Lopez-Sanchez, A. Sahuquillo, R. Rubio, C. Davidson, A. Ure, and P. Quevauviller. 1999. “Improvement of the BCR three step sequential extraction procedure prior to the certification of new sediment and soil reference materials.” J. Environ. Monit. 1 (1): 57–61. https://doi.org/10.1039/a807854h.
Reddy, V. A., C. H. Solanki, S. Kumar, K. R. Reddy, and Y. J. Du. 2019. “New ternary blend limestone calcined clay cement for solidification/stabilization of zinc contaminated soil.” Chemosphere 235: 308–315. https://doi.org/10.1016/j.chemosphere.2019.06.051.
Saikia, N. J., P. Sengupta, P. K. Gogoi, and P. C. Borthakur. 2002. “Hydration behaviour of lime-co-calcined kaolin-petroleum effluent treatment plant sludge.” Cem. Concr. Res. 32 (2): 297–302. https://doi.org/10.1016/S0008-8846(01)00676-7.
Ščančar, J., M. Strazar, and O. Burica. 2000. “Total metal concentrations and partitioning of Cd, Cr, Cu, Fe, Ni and Zn in sewage sludge.” Sci. Total Environ. 250 (1–3): 9–19. https://doi.org/10.1016/S0048-9697(99)00478-7.
Sharma, H. D., and K. R. Reddy. 2004. Geoenvironmental engineering: Site remediation, waste containment, and emerging waste management technologies. Hoboken, NJ: Wiley.
Singh, T. S., and K. K. Pant. 2006. “Solidification/stabilization of arsenic containing solid wastes using portland cement, fly ash and polymeric materials.” J. Hazard. Mater. 131 (1–3): 29–36. https://doi.org/10.1016/j.jhazmat.2005.06.046.
Sinha, A. K., V. G. Havanagi, and J. T. Shahu. 2019. “Construction and performance of jarofix waste material embankment.” Proc. Inst. Civ. Eng. Constr. Mater. 1–16. https://doi.org/10.1680/jcoma.18.00003.
Suh, J. I., W. S. Yum, Y. Jeong, H. G. Park, and J. E. Oh. 2019. “The cation-dependent effects of formate salt additives on the strength and microstructure of CaO-activated fly ash binders.” Constr. Build. Mater. 194: 92–101. https://doi.org/10.1016/j.conbuildmat.2018.11.008.
Tessier, A., P. G. Campbell, and M. Bisson. 1979. “Sequential extraction procedure for the speciation of particulate trace metals.” Anal. Chem. 51 (7): 844–851. https://doi.org/10.1021/ac50043a017.
USEPA. 1992. Toxicity characteristic leaching procedure (TCLP), 1–35. Method 1311. Washington, DC: USEPA.
Voglar, G. E., and D. Leštan. 2010. “Solidification/stabilisation of metals contaminated industrial soil from former Zn smelter in Celje, Slovenia, using cement as a hydraulic binder.” J. Hazard. Mater. 178 (1–3): 926–933. https://doi.org/10.1016/j.jhazmat.2010.02.026.
Wang, F., Y. Zhang, Z. Shen, H. Pan, J. Xu, and A. Al-Tabba. 2019a. “GMCs stabilized/solidified Pb/Zn contaminated soil under different curing temperature: Leachability and durability.” Environ. Sci. Pollut. Res. 26 (26): 26963–26971. https://doi.org/10.1007/s11356-019-05894-5.
Wang, L., D.-W. Cho, D. C. W. Tsang, X. Cao, D. Hou, Z. Shen, D. S. Alessi, Y. Sik, and C. Sun. 2019b. “Green remediation of As and Pb contaminated soil using cement-free clay-based stabilization/solidification.” Environ. Int. 126: 336–345. https://doi.org/10.1016/j.envint.2019.02.057.
Wang, Q., S. Li, S. Pan, X. Cui, D. J. Corr, and S. P. Shah. 2019c. “Effect of graphene oxide on the hydration and microstructure of fly ash-cement system.” Constr. Build. Mater. 198: 106–119. https://doi.org/10.1016/j.conbuildmat.2018.11.199.
Wu, M., Y. Zhang, Y. Jia, W. She, G. Liu, Z. Wu, and W. Sun. 2019. “Influence of sodium hydroxide on the performance and hydration of lime-based low carbon cementitious materials.” Constr. Build. Mater. 200: 604–615. https://doi.org/10.1016/j.conbuildmat.2018.12.102.
Xia, M., F. Muhammad, L. Zeng, S. Li, X. Huang, B. Jiao, Y. C. Shiau, and D. Li. 2019. “Solidification/stabilization of lead-zinc smelting slag in composite based geopolymer.” J. Cleaner Prod. 209: 1206–1215. https://doi.org/10.1016/j.jclepro.2018.10.265.
Xia, W.-Y., Y.-S. Feng, Y.-J. Du, K. R. Reddy, and M.-L. Wei. 2018. “Solidification and stabilization of heavy metal–contaminated industrial site soil using KMP binder.” J. Mater. Civ. Eng. 30 (6): 04018080. https://doi.org/10.1061/(ASCE)MT.1943-5533.0002264.
Xia, W. Y., Y. S. Feng, F. Jin, L. M. Zhang, and Y. J. Du. 2017. “Stabilization and solidification of a heavy metal contaminated site soil using a hydroxyapatite based binder.” Constr. Build. Mater. 156: 199–207. https://doi.org/10.1016/j.conbuildmat.2017.08.149.
Zhang, C., X. Min, J. Zhang, M. Wang, Y. Li, and J. Fei. 2016. “Reductive clean leaching process of cadmium from hydrometallurgical zinc neutral leaching residue using sulfur dioxide.” J. Cleaner Prod. 113: 910–918. https://doi.org/10.1016/j.jclepro.2015.11.059.
Zhang, Z., G. Guo, Y. Teng, J. Wang, J. S. Rhee, S. Wang, and F. Li. 2015. “Screening and assessment of solidification/stabilization amendments suitable for soils of lead-acid battery contaminated site.” J. Hazard. Mater. 288: 140–146. https://doi.org/10.1016/j.jhazmat.2015.02.015.

Information & Authors

Information

Published In

Go to Journal of Hazardous, Toxic, and Radioactive Waste
Journal of Hazardous, Toxic, and Radioactive Waste
Volume 24Issue 4October 2020

History

Received: Mar 22, 2020
Accepted: May 18, 2020
Published online: Jul 30, 2020
Published in print: Oct 1, 2020
Discussion open until: Dec 30, 2020

Permissions

Request permissions for this article.

Authors

Affiliations

Ph.D. Student, Civil Engineering Dept., Sardar Vallabhbhai National Institute of Technology, Surat 395007, Gujarat, India (corresponding author). ORCID: https://orcid.org/0000-0002-2210-2273. Email: [email protected]
Chandresh H. Solanki [email protected]
Professor, Civil Engineering Dept., Sardar Vallabhbhai National Institute of Technology, Surat 395007, Gujarat, India. Email: [email protected]
Shailendra Kumar [email protected]
Assistant Professor, Civil Engineering Dept., Sardar Vallabhbhai National Institute of Technology, Surat 395007, Gujarat, India. Email: [email protected]
Professor, Dept. of Civil and Materials Engineering, Univ. of Illinois at Chicago, Chicago, IL 60607. ORCID: https://orcid.org/0000-0002-6577-1151. Email: [email protected]
Professor, Jiangsu Key Laboratory of Urban Underground Engineering & Environmental Safety, Institute of Geotechnical Engineering, Southeast Univ., Nanjing 210096, China. Email: [email protected]

Metrics & Citations

Metrics

Citations

Download citation

If you have the appropriate software installed, you can download article citation data to the citation manager of your choice. Simply select your manager software from the list below and click Download.

Cited by

View Options

Get Access

Access content

Please select your options to get access

Log in/Register Log in via your institution (Shibboleth)
ASCE Members: Please log in to see member pricing

Purchase

Save for later Information on ASCE Library Cards
ASCE Library Cards let you download journal articles, proceedings papers, and available book chapters across the entire ASCE Library platform. ASCE Library Cards remain active for 24 months or until all downloads are used. Note: This content will be debited as one download at time of checkout.

Terms of Use: ASCE Library Cards are for individual, personal use only. Reselling, republishing, or forwarding the materials to libraries or reading rooms is prohibited.
ASCE Library Card (5 downloads)
$105.00
Add to cart
ASCE Library Card (20 downloads)
$280.00
Add to cart
Buy Single Article
$35.00
Add to cart

Get Access

Access content

Please select your options to get access

Log in/Register Log in via your institution (Shibboleth)
ASCE Members: Please log in to see member pricing

Purchase

Save for later Information on ASCE Library Cards
ASCE Library Cards let you download journal articles, proceedings papers, and available book chapters across the entire ASCE Library platform. ASCE Library Cards remain active for 24 months or until all downloads are used. Note: This content will be debited as one download at time of checkout.

Terms of Use: ASCE Library Cards are for individual, personal use only. Reselling, republishing, or forwarding the materials to libraries or reading rooms is prohibited.
ASCE Library Card (5 downloads)
$105.00
Add to cart
ASCE Library Card (20 downloads)
$280.00
Add to cart
Buy Single Article
$35.00
Add to cart

Media

Figures

Other

Tables

Share

Share

Copy the content Link

Share with email

Email a colleague

Share