Abstract
This paper was presented in part by V. L. Snoeyink as the Simon W. Freese Lecture at the 2002 Canadian Society of Civil Engineers/Environmental and Water Resources Institute of ASCE Environmental Engineering Conference in Niagara Falls, Ontario, Canada, July 22, 2002. The interactions of corroded iron pipe surfaces with water are of importance because they can lead to serious water quality degradation and material deterioration. A conceptual model has been developed in this paper to describe the formation and growth of iron scales, and their reactions that lead to colored water problems. Most corrosion scales have characteristic structural features, such as a loosely held top surface layer, a shell-like layer(s), and a porous core. According to this model corrosion scales are expected to grow from inside the scale via the corrosion reaction, i.e., the conversion of iron metal to ferrous ion. The average oxidation state of iron increases with distance from the pipe wall. The scale structure and scale reactions permit the ferrous iron to be released to the bulk water, where it undergoes conversion to particulate ferric iron, which is the cause of colored water. Scale structure and composition play important roles in the reactions of iron scales that lead to iron release, and water quality control to decrease the porosity of the scale is an important means of reducing iron release. It is anticipated that the conceptual model presented here will be used as a basis for changing water quality to minimize colored water formation, and as a guide for further research.
Get full access to this article
View all available purchase options and get full access to this article.
References
Baylis, J. R.(1926). “Prevention of corrosion and red water.” J. Am. Water Works Assoc., 15(6), 598–631.
Benjamin, M. M., Sontheimer, H., and Leroy, P. (1996). “Corrosion of iron and steel.” Internal corrosion of water distribution systems, AWWA Research Foundation, Denver, 29–70.
Carlson, L., and Schwertmann, U.(1990). “The effect of and oxidation rate on the formation of goethite versus lepidocrocite from an Fe(II) system at ph 6 and 7.” Clay Miner., 25, 65–71.
Clement, J. A. et al. (2002). “Development of red water control strategies.” Technical Rep., AWWA Research Foundation, Denver.
Cornell, R. M., Schneider, W., and Giovanoli, R.(1989). “Phase transformations in the ferrihydrite/cysteine system.” Polyhedron, 8, 2829–2834.
Cornell, R. M., and Schwertmann, U. (1996). The iron oxides, VCH, New York.
Daniels, L., Negash, B., Rajagopal, B. S., and Weimer, P. J.(1987). “Bacterial methanogenesis and growth from with elemental iron as the sole source of electrons.” Science, 237(4814), 509–511.
Drissi, H., Refait, P., and Génin, J. M. R.(1994). “The oxidation of in the presence of carbonate ions: structure of carbonate green rust one.” Hyperfine Interact., 90, 1–4.
Drissi, S. H., Refait, P., Abdelmoula, M., and Génin, J. M. R.(1995). “Preparation and thermodynamic properties of Fe(II)–Fe(III) hydroxide–carbonate (green rust 1); Pourbaix diagram of iron in carbonate-containing aqueous media.” Corros. Sci., 37, 2025–2041.
Evans, U. R.(1965). “Electrochemical mechanism of atmospheric rusting.” Nature (London), 206, 980–982.
Evans, U. R., and Taylor, C. A. J.(1972). “Mechanism of atmospheric rusting.” Corros. Sci., 12, 227–246.
Fischer, W. R.(1987). “Standard potentials of iron (III) oxides under reducing conditions.” Z. Pflanzenernaehr. und Bodenkd., 150, 286–289.
Génin, J.-M. R., Refait, P., Simon, L., and Drissi, S. H.(1997). “Preparation and E/sub h/-pH diagrams of Fe(II)–Fe(III) green rust compounds; hyperfine interaction characteristics and stoichiometry of hydroxy-chloride, -sulphate and -carbonate.” Hyperfine Interact., 111, 313–318.
Golden, D. C., and Dixon, J. B.(1985). “Silicate and phosphate influence on kaolin–iron oxide interactions.” Soil Sci. Soc. Am. J., 49, 1568–1575.
Herro, H. M., and Port, R. D. (1993). The Nalco guide to cooling water system failure analysis, McGraw-Hill, New York.
Karim, Z.(1984). “Characteristics of ferrihydrites formed by oxidation of solutions containing different amounts of silica.” Clays Clay Miner., 32, 181–184.
Kölle, W., and Rosch, H.(1980). “Untersuchungen an Rohrnetz-Inkrustierungen unter mineralogischen Gesichtspunkten.” Vom Wasser, 55, 159–178.
Kuch, A.(1988). “Investigations of the reduction and re-oxidation kinetics of iron (III) oxide scales formed in waters.” Corros. Sci., 28(3), 221–231.
Larson, T. E., and King, R. M.(1954). “Corrosion by water at low flow velocity.” J. Am. Water Works Assoc., 46, 1–9.
Larson, T. E., and Skold, R. V.(1957). “Corrosion and tuberculation of cast iron.” J. Am. Water Works Assoc., 9(10), 1294–1302.
Lorowitz, W. H., Nagle, D. P., Jr., and Tanner, R. S.(1992). “Anaerobic oxidation of elemental metals coupled to methanogenesis by methanobacterium thermoautotrophicum.” Environ. Sci. Technol., 26(8), 1606–1610.
Millero, F. J., Sotolongo, S., and Izaguirre, M.(1987). “The oxidation kinetics of Fe(II) in seawater.” Geochim. Cosmochim. Acta, 51, 793–801.
Montgomery, J. M. (1985). Water treatment principles and design, Wiley, New York.
Obrecht, M. F., and Pourbaix, M.(1967). “Corrosion of metals in potable water systems.” J. Am. Water Works Assoc., 59, 977–992.
Olowe, A. A., Génin, J. M. R., and Bauer, P.(1988). “Hyperfine interactions and structures of ferrous hydroxide and green rust II in sulfated aqueous media.” Hyperfine Interact., 41, 501–504.
Pryor, M. J., and Cohen, M.(1951a). “The mechanism of the inhibition of the corrosion of iron by solutions of sodium orthophosphate.” J. Electrochem. Soc., 98(7), 263–272.
Pryor, M. J., and Cohen, M.(1951b). “Role of dissolved oxygen during the inhibition of the corrosion of iron by sodium phosphate solutions.” Nature (London), 167, 157.
Pryor, M. J., and Cohen, M.(1953). “The inhibition of iron by some anodic inhibitors.” J. Electrochem. Soc., 100(5), 203–215.
Pryor, M. J., Cohen, M., and Brown, F.(1952). “The nature of the films formed by passivation of iron with solutions of sodium phosphate.” J. Electrochem. Soc., 99(12), 542–545.
Refait, P., Abdelmoula, M., and Génin, J. M.(1998). “Mechanisms of formation and structure of Green Rust one in aqueous corrosion of iron in the presence of chloride ions.” Corros. Sci., 40(9), 1547–1560.
Sarin P., Snoeyink V. L., Bebee J., Jim K. K., Beckett M. A., Kriven W. M., and Clement J. A. (2002a). “Iron release from ‘Old’ iron pipes used in drinking water distribution systems: Effect of dissolved oxygen.” Water Res., in press.
Sarin, P., Snoeyink, V. L., Bebee, J., Kriven, W. M., and Clement, J. A.(2001). “Physico-chemical characteristics of corrosion scales in old iron pipes.” Water Res., 35, 2961–2969.
Sarin, P., Snoeyink, V. L., Clement, J. A., and Kriven, W. M.(2002b). “Iron release from corroded unlined cast iron pipe: Effect of pH, alkalinity, and orthophosphates in a soft New England water.” J. Am. Water Works Assoc., 95(11), 85–96.
Schwertmann, U., and Taylor, R. M. (1977). “Iron oxides.” Minerals in soil environments, S. B. Weed, ed., Soil Science Society of America, Madison, Wis., 145–179.
Schwertmann, U., and Thalmann, H.(1976). “The influence of Fe(II), Si, and pH on the formation of lepidocrocite and ferrihydrite during oxidation of aqueous solutions.” Clay Miner., 11, 189–200.
Sontheimer, H., Benjamin, M. M., and Leroy, P. (1985). “Corrosion of iron and steel.” Internal corrosion of water distribution systems, AWWA Research Foundation, Denver.
Sontheimer, H., Kolle, W., and Snoeyink, V. L.(1981). “The siderite model of the formation of corrosion-resistant scales.” J. Am. Water Works Assoc., 73(11), 572–579.
Stratmann, M., Bohnenkamp, K., and Engell, H.-J.(1983). “An electrochemical study of phase-transitions in rust layers.” Corros. Sci., 23(9), 969–985.
Stratmann, M., and Hoffmann, K.(1989). “In situ Mossbauer spectroscopic study of reactions within rust layers.” Corros. Sci., 29(11/12), 1329–1352.
Stratmann, M., and Muller, J.(1994). “The mechanism of the oxygen reduction on rust-covered metal substrates.” Corros. Sci., 36(2), 327–359.
Stumm, W., and Lee, G. F.(1961). “Oxygenation of ferrous iron.” Ind. Eng. Chem., 53(2), 143–146.
Sung, W., and Morgan, J.(1980). “Kinetics and product of ferrous iron oxygenation in aqueous systems.” Environ. Sci. Technol., 14(5), 561–568.
Tamaura, Y., Buduan, P. V., and Katsura, T.(1981). “Studies on the oxidation of iron(II) ion during the formation of and α-FeO(OH) by air oxidation of suspensions.” J. Chem. Soc. Dalton Trans., 9, 1807–1811.
Tamura, H., Gato, K., and Nagayama, M.(1976). “Effect of anions on the oxygenation of ferrous ion in neutral solutions.” J. Inorg. Nucl. Chem., 38, 113–117.
Taylor, R. M.(1984). “Influence of chloride on the formation of iron oxides from Fe(II) chloride. Effect of (Cl) on the formation of lepidocrocite and its crystallinity.” Clays Clay Miner., 32, 175–180.
Vik, E. A., Ryder, R. A., Wagner, I., and Ferguson, J. F. (1996). “Mitigation of corrosion effects.” Internal corrosion of water distribution systems, V. L. Snoeyink, ed., AWWA Research Foundation, Denver, 389–443.
Von Gunten, U., and Schneider, W.(1991). “Primary products of the oxygenation of iron(II) at an oxic-anoxic boundary. Nucleation, aggregation, and aging.” J. Colloid Interface Sci., 145, 127–139.
Information & Authors
Information
Published In
Copyright
Copyright © 2004 American Society of Civil Engineers.
History
Received: Jan 24, 2003
Accepted: May 14, 2003
Published online: Mar 15, 2004
Published in print: Apr 2004
Authors
Metrics & Citations
Metrics
Citations
Download citation
If you have the appropriate software installed, you can download article citation data to the citation manager of your choice. Simply select your manager software from the list below and click Download.