Performance of Self-Healed Alkali-Activated Slag Mortar at Elevated Temperature
Publication: Journal of Materials in Civil Engineering
Volume 35, Issue 7
Abstract
Microbially induced calcium carbonate precipitation (MICP) is a novel technology aimed at improving the strength and durability of concrete by using micro-organism species. This paper investigated the influence of the bacterial treatment on the strength parameters and microstructures of alkali-activated slag (AAS) mortars at elevated temperatures. Four AAS mortar mixtures containing varying concentrations of Bacillus pasteurii (, , and ) were investigated at target temperatures of 23°C, 200°C, 400°C, 600°C, and 800°C. After reaching the target temperature, mass loss, compressive strength, and flexural strength tests were carried out on the specimens. Scanning electron microscopy (SEM), X-ray spectroscopy (EDS), and X-ray diffraction (XRD) tests were conducted to compare the microstructure characteristics of bacteria-containing mortars and the control mortar. The results showed a substantial increase of compressive and flexural strength of AAS mortars at ambient and elevated temperatures. In addition, the microstructure analysis indicated that the bacterial specimens produced calcite, leading to crack healing and improvement of mechanical properties; this confirms the functionality and viability of incorporating Bacillus pasteurii in the alkaline environment of AAS mortars.
Get full access to this article
View all available purchase options and get full access to this article.
Data Availability Statement
The data sets used and/or analyzed in this study are available from the corresponding author upon reasonable request.
Acknowledgments
The authors thank Islamic Azad University of Najafabad for the research facilities.
References
Achal, V., A. Mukerjee, and M. Sudhakara Reddy. 2013. “Biogenic treatment improves the durability and remediates the cracks of concrete structures.” Constr. Build. Mater. 48 (Nov): 1–5. https://doi.org/10.1016/j.conbuildmat.2013.06.061.
Al-Salloum, Y., H. Abbas, Q. I. Sheikh, S. Hadi, S. Alsayed, and T. Almusallam. 2017. “Effect of some biotic factors on microbially-induced calcite precipitation in cement mortar.” Saudi J. Biol. Sci. 24 (2): 286–294. https://doi.org/10.1016/j.sjbs.2016.01.016.
Andalib, R., M. Zaimi, M. Z. Abd Majid, M. Hussin, A. Keyvanfar, A. Talaiekhozani, and H. Haidar. 2015. “Geo-polymer bacterial concrete using microorganism.” J. Environ. Treat. Tech. 3 (4): 212–214.
ASTM. 2016. Standard test method for compressive strength of hydraulic cement mortars (using 2-in. or [50-mm] cube specimens). ASTM C109. West Conshohocken, PA: ASTM.
ASTM. 2018. Standard test method for flexural strength of hydraulic-cement mortars. ASTM C348. West Conshohocken, PA: ASTM.
Awoyera, P., and A. Adesina. 2019. “A critical review on application of alkali activated slag as a sustainable composite binder.” Case Stud. Constr. Mater. 11 (Dec): e00268. https://doi.org/10.1016/j.cscm.2019.e00268.
Bastani, M., and K. Behfarnia. 2020. “Application of alkali-activated slag in roller compacted concrete.” Int. J. Pavement Res. Technol. 13 (3): 324–333. https://doi.org/10.1007/s42947-020-0088-y.
Behfarnia, K., and M. Shahbaz. 2018. “The effect of elevated temperature on the residual tensile strength and physical properties of the alkali-activated slag concrete.” J. Build. Eng. 20 (Nov): 442–454. https://doi.org/10.1016/j.jobe.2018.08.015.
Behnood, A., and H. Ziari. 2008. “Effects of silica fume addition and water to cement ratio on the properties of high-strength concrete after exposure to high temperatures.” Cem. Concr. Compos. 30 (2): 106–112. https://doi.org/10.1016/j.cemconcomp.2007.06.003.
Çelikten, S., M. Sarıdemir, and İ. Özgür Deneme. 2019. “Mechanical and microstructural properties of alkali-activated slag and slag + fly ash mortars exposed to high temperature.” Constr. Build. Mater. 217 (Aug): 50–61. https://doi.org/10.1016/j.conbuildmat.2019.05.055.
Chahal, N., R. Siddique, and A. Rajor. 2012. “Influence of bacteria on the compressive strength, water absorption and rapid chloride permeability of fly ash concrete.” Constr. Build. Mater. 28 (1): 351–356. https://doi.org/10.1016/j.conbuildmat.2011.07.042.
De Muynck, W., D. Debrouwer, N. De Belie, and W. Verstraete. 2008. “Bacterial carbonate precipitation improves the durability of cementitious materials.” Cem. Concr. Res. 38 (7): 1005–1014. https://doi.org/10.1016/j.cemconres.2008.03.005.
Ding, Y., J.-G. Dai, and C.-J. Shi. 2016. “Mechanical properties of alkali-activated concrete: A state-of-the-art review.” Constr. Build. Mater. 127 (Nov): 68–79. https://doi.org/10.1016/j.conbuildmat.2016.09.121.
Douglas, E., A. Bilodeau, and V. M. Malhotra. 1992. “Properties and durability of alkali-activated slag concrete.” Mater. J. 89 (5): 509–516.
Edvardsen, C. 1999. “Water permeability and autogenous healing of cracks in concrete.” In Innovation in concrete structures: Design and construction, 473–487. London: Institution of Civil Engineers.
Guerrieri, M., and J. Sanjayan. 2011. “Investigation of the cause of disintegration of alkali-activated slag at temperature exposure of 50°C.” J. Mater. Civ. Eng. 23 (12): 1589–1595. https://doi.org/10.1061/(ASCE)MT.1943-5533.0000313.
Habert, G., J. B. d’Espinose de Lacaillerie, and N. Roussel. 2011. “An environmental evaluation of geopolymer based concrete production: Reviewing current research trends.” J. Cleaner Prod. 19 (11): 1229–1238. https://doi.org/10.1016/j.jclepro.2011.03.012.
Hajek, P. 2017. “Concrete structures for sustainability in a changing world.” Procedia Eng. 171 (2017): 207–214. https://doi.org/10.1016/j.proeng.2017.01.328.
Hosseini Balam, N., D. Mostofinejad, and M. Eftekhar. 2017a. “Effects of bacterial remediation on compressive strength, water absorption, and chloride permeability of lightweight aggregate concrete.” Constr. Build. Mater. 145 (Aug): 107–116. https://doi.org/10.1016/j.conbuildmat.2017.04.003.
Hosseini Balam, N., D. Mostofinejad, and M. Eftekhar. 2017b. “Use of carbonate precipitating bacteria to reduce water absorption of aggregates.” Constr. Build. Mater. 141 (Jun): 565–577. https://doi.org/10.1016/j.conbuildmat.2017.03.042.
Husem, M. 2006. “The effects of high temperature on compressive and flexural strengths of ordinary and high-performance concrete.” Fire Saf. J. 41 (2): 155–163. https://doi.org/10.1016/j.firesaf.2005.12.002.
Imbabi, M. S., C. Carrigan, and S. McKenna. 2012. “Trends and developments in green cement and concrete technology.” Int. J. Sustainable Built Environ. 1 (2): 194–216. https://doi.org/10.1016/j.ijsbe.2013.05.001.
Jadhav, U. U., M. Lahoti, Z. Chen, J. Qiu, B. Cao, and E.-H. Yang. 2018. “Viability of bacterial spores and crack healing in bacteria-containing geopolymer.” Constr. Build. Mater. 169 (Apr): 716–723. https://doi.org/10.1016/j.conbuildmat.2018.03.039.
Janštová, B., and J. Lukášová. 2001. “Heat resistance of Bacillus spp. spores isolated from cow’s milk and farm environment.” Acta Veterinaria Brno 70 (2): 179–184. https://doi.org/10.2754/avb200170020179.
Jonkers, H. M., A. Thijssen, G. Muyzer, O. Copuroglu, and E. Schlangen. 2010. “Application of bacteria as self-healing agent for the development of sustainable concrete.” Ecol. Eng. 36 (2): 230–235. https://doi.org/10.1016/j.ecoleng.2008.12.036.
Khaliq, W., and M. B. Ehsan. 2016. “Crack healing in concrete using various bio influenced self-healing techniques.” Constr. Build. Mater. 102 (Part 1): 349–357. https://doi.org/10.1016/j.conbuildmat.2015.11.006.
Khaliq, W., and F. Waheed. 2017. “Mechanical response and spalling sensitivity of air entrained high-strength concrete at elevated temperatures.” Constr. Build. Mater. 150 (Sep): 747–757. https://doi.org/10.1016/j.conbuildmat.2017.06.039.
Khitab, A., M. Arshad, A. Ffaisal, and I. Khan. 2013. “Development of an acid resistant concrete: A review.” Int. J. Sustainable Constr. Eng. Technol. 4 (2): 33–38.
Madlool, N. A., R. Saidur, M. S. Hossain, and N. A. Rahim. 2011. “A critical review on energy use and savings in the cement industries.” Renewable Sustainable Energy Rev. 15 (4): 2042–2060. https://doi.org/10.1016/j.rser.2011.01.005.
McKelvey, D., V. Sivakumar, A. Bell, and G. McLaverty. 2002. “Shear strength of recycled construction materials intended for use in vibro ground improvement.” Proc. Inst. Civ. Eng. Ground Improv. 6 (2): 59–68. https://doi.org/10.1680/grim.2002.6.2.59.
Metwally, G. A., M. G. Mahdy, and A. H. El-Raheem. 2020. “Effectiveness of Bacillus pasteurii on properties of self-healing concrete.” J. Mech. Civ. Eng. 17 (1): 13–22. https://doi.org/10.9790/1684-1701041322.
Mohamad, N., K. Muthusamy, R. Embong, A. Kusbiantoro, and M. H. Hashim. 2022. “Environmental impact of cement production and Solutions: A review.” Mater. Today: Proc. 48 (Part 4): 741–746. https://doi.org/10.1016/j.matpr.2021.02.212.
Mohamed, O. A. 2019. “A review of durability and strength characteristics of alkali-activated slag concrete.” Materials 12 (8): 1198. https://doi.org/10.3390/ma12081198.
Mondal, S., and A. D. Ghosh. 2018. “Investigation into the optimal bacterial concentration for compressive strength enhancement of microbial concrete.” Constr. Build. Mater. 183 (Sep): 202–214. https://doi.org/10.1016/j.conbuildmat.2018.06.176.
Nain, N., R. Surabhi, N. V. Yathish, V. Krishnamurthy, T. Deepa, and S. Tharannum. 2019. “Enhancement in strength parameters of concrete by application of Bacillus bacteria.” Constr. Build. Mater. 202 (Mar): 904–908. https://doi.org/10.1016/j.conbuildmat.2019.01.059.
Qiu, J., D. Q. S. Tng, and E.-H. Yang. 2014. “Surface treatment of recycled concrete aggregates through microbial carbonate precipitation.” Constr. Build. Mater. 57 (Apr): 144–150. https://doi.org/10.1016/j.conbuildmat.2014.01.085.
Reddy, M. A. 2016. “Temperature effect on various bacteria used in microbial concrete.” Int. J. Innovative Res. Sci. Eng. Technol. 5 (4): 5083–5090. https://doi.org/10.15680/IJIRSET.2016.0504098.
Rovnaník, P., and Á. Dufka. 2015. “Effect of the aggregate type on the properties of alkali-activated slag subjected to high temperatures.” Mater. Tech. 49 (5): 709–713.
Sedaghatdoost, A., K. Behfarnia, M. Bayati, and M. S. Vaezi. 2019. “Influence of recycled concrete aggregates on alkali-activated slag mortar exposed to elevated temperatures.” J. Build. Eng. 26 (Nov): 100871. https://doi.org/10.1016/j.jobe.2019.100871.
Singh, L. P., V. Bisht, M. S. Aswathy, L. Chaurasia, and S. Gupta. 2018. “Studies on performance enhancement of recycled aggregate by incorporating bio and nano materials.” Constr. Build. Mater. 181 (Aug): 217–226. https://doi.org/10.1016/j.conbuildmat.2018.05.248.
Türker, H. T., M. Balçikanli, İ. H. Durmuş, E. Özbay, and M. Erdemir. 2016. “Microstructural alteration of alkali activated slag mortars depend on exposed high temperature level.” Constr. Build. Mater. 104: 169–180. https://doi.org/10.1016/j.conbuildmat.2015.12.070.
Vaezi, M., S. A. Zareei, and M. Jahadi. 2020. “Recycled microbial mortar: Effects of bacterial concentration and calcium lactate content.” Constr. Build. Mater. 234 (Feb): 117349. https://doi.org/10.1016/j.conbuildmat.2019.117349.
Wardhono, A., D. W. Law, and A. Strano. 2015. “The strength of alkali-activated slag/fly ash mortar blends at ambient temperature.” Procedia Eng. 125: 650–656. https://doi.org/10.1016/j.proeng.2015.11.095.
Worrell, E., N. Martin, and L. Price. 2000. “Potentials for energy efficiency improvement in the US cement industry.” Energy 25 (12): 1189–1214. https://doi.org/10.1016/S0360-5442(00)00042-6.
Information & Authors
Information
Published In
Copyright
© 2023 American Society of Civil Engineers.
History
Received: Dec 4, 2021
Accepted: Nov 8, 2022
Published online: Apr 24, 2023
Published in print: Jul 1, 2023
Discussion open until: Sep 24, 2023
Authors
Metrics & Citations
Metrics
Citations
Download citation
If you have the appropriate software installed, you can download article citation data to the citation manager of your choice. Simply select your manager software from the list below and click Download.