Abstract

EN 934-2 “Admixtures for concrete, mortar and grout Concrete admixtures. Definitions, requirements, conformity, marking and labelling” requires that any increase in the air content shall not be more than 2% by volume over that obtained from the reference mix, and most types of superplasticizers (SPs) easily meet this requirement. Some types may even reduce the level of air, and this can result in a less cohesive mix, which may be more prone to bleed and segregation or may leave the mix feeling harsh and difficult to handle. Unfortunately, some types of superplasticizers increase the level of air. Too high a volume of air has been overcome using an antifoaming agent. The influence of new-generation type superplasticizer and antifoaming admixture (AFA) on the air content and workability of high performance self-compacting concrete (HPSCC) is analyzed in this paper. The purpose of this study was to examine the influence of the admixture type on pore size distribution, compressive strength and frost resistance of HPSCC at constant water to cement ratio, type and volume of aggregate, and volume of cement paste. The parameters of the open pores and air voids of hardened HPSCC are also investigated. The results presented in this paper show that admixtures significantly influence the investigated properties of HPSCC.

Get full access to this article

View all available purchase options and get full access to this article.

References

ACI. (2008). “Guide to durable concrete.”.
Aïtcin, P.-C. (1998). “The influence of the spacing factor on the freeze-thaw durability of high performance concrete.” Int. Symp. of High-Performance and Reactive Power Concretes, Sherbrooke, QC, Canada.
ASTM. (2008). “Standard test method for resistance of concrete to rapid freezing and thawing.” C666/C666M-03, Reston, VA.
ASTM. (2014). Standard test method for air content of freshly mixed concrete by the pressure method.” C231/C231M-14, West Conshohocken, PA.
Austrian Standard. (2002). “Beton. Teil 1: Festlegung, Herstellung, Verwendung und. Konformitätsnachweis.”.
British Standards Institution (BSI). (2003). “Concrete—Part 1: Specification, performance, production and conformity.”, London.
British Standards Institution (BSI). (2008). “Admixtures for concrete, mortar and grout—Test methods—Part 11: Determination of air void characteristics in hardened concrete.”, London.
British Standards Institution (BSI). (2009a). “Testing fresh concrete. Air content. Pressure methods.”, London.
British Standards Institution (BSI). (2009b). “Testing hardened concrete. Compressive strength of test specimens.”, London.
British Standards Institution (BSI). (2010). “Testing fresh concrete—Part 8: Self-compacting concrete—Slump-flow test.”, London.
British Standards Institution (BSI). (2012). “Admixtures for concrete, mortar and grout. Concrete admixtures. Definitions, requirements, conformity, marking and labelling.”, London.
Danish Standard. (2004). “Concrete Materials—Rules for application.”, Denmark.
Fagerlund, G. (1999). Durability of concrete structures, Arkady, Warsaw, Poland.
Fang, Y., Wang, R., Pang, E., and Zhou, Y. (2010). “Relationship between compressive strength and air-void structure of foamed cement-fly ash concrete.” J. Chin Ceram. Soc., 38(4), 621–626.
Federal Ministry of Transport. (2001). “Additional technical terms of contract and guidelines for the construction of pavements.”, FSGV, Cologne.
Felekoğlu, B., Türkel, S., and Baradan, B. (2007). “Effect of water/cement ratio on the fresh and hardened properties of self-compacting concrete.” Build. Environ., 42(4), 1795–1802.
Foy, C., Pigeon, M., and Bathia, N. (1988). “Freeze-thaw durability and deicer salt scaling resistance of a 0.25 water-cement ratio concrete.” Cem. Concr. Res., 18(4), 604–614.
Glinicki, M. A. (2005). “European requirements for air-entrained concrete in XF class environment.” Drogownictwo, 3, 86–88.
Grodzicka, A. (2005). Frost resistance of high performance concrete, Wydawnictwa Instytutu Techniki Budowlanej, Warsaw, Poland.
Hanehara, S., and Yamada, K. (2008). “Rheology and early age properties of cement systems.” Cem. Concr. Res., 38(2), 175–195.
Jacobsen, S., Sœther, D. H., and Sellevold, E. J. (1997). “Frost testing of high strength concrete: Frost/salt scaling at different cooling rates.” Mater. Struct., 30(1), 33–42.
Kearsley, E. P., and Wainwright, P. J. (2002). “The effect of porosity on the strength of foamed concrete.” Cem. Concr. Res., 32(2), 233–239.
Khatib, J. M., and Mangat, P. S. (1999). “Influence of superplasticizer and curing on porosity and pore structure of cement paste.” Cem. Concr. Compos., 21(5–6), 431–437.
Khayat, K. H., and Assaad, J. (2002). “Air-void stability in self-consolidating concrete.” Mater. J., 99(4), 408–416.
Łaźniewska-Piekarczyk, B. (2010). “Influence of anti-foaming admixture and polycarboxylic superplasticizer type on fresh and hardened properties of self-compacting mortar.” Archit. Civ. Eng. Environ., 3(4), 61–72.
Łaźniewska-Piekarczyk, B. (2012). “The influence of selected new generation admixtures on the workability, air-voids parameters and frost-resistance of self compacting concrete.” Constr. Build. Mater., 31, 310–319.
Łaźniewska-Piekarczyk, B. (2013) “The influence of selected new generation admixtures on the workability, air-voids parameters and frost-resistance of self compacting concrete.” Constr. Build. Mater., 40, 659–671.
Łaźniewska-Piekarczyk, B., and Szwabowski, J. (2012). “Anti-foaming admixture (AFA) and its influences on the properties of a fresh self-compacting concrete mix.” J. Civ. Eng. Manage., 18(2), 151–157.
MacInnis, C., and Racic, D. (1986). “The effect of superplasticizers on the entrained air-void system in concrete.” Cem. Concr. Res., 16(3), 345–352.
Meyer, F. (1998). “Air void distribution in concrete for the great belt link, West Bridge.” Nordic Concrete Research, 17.
Mielenz, R. C., Wolkodoff, V. E., Backstrom, J. E., and Burrows, R. H. (1958). “Origin, evolution, and effects of the air void system in concrete. Part 4—The air void system and job concrete.” Proc. Am. Concr. Inst., 55, 507–517.
Mosquet, M. (2003). The new generation admixtures, Vol. 2, Budownictwo Technologie Architektura, 21–23.
Odler, I., and Robler, M. (1985). “Investigation on the relationship between porosity, structure and strength of hydrated portland cement paste. (II) Effect of pore structure and of degree of hydration.” Cem. Concr. Res., 15(3), 401–410.
Philleo, R. E. (1987). “Frost susceptibility of high-strength concrete.” Concrete Durability—Katharine and Bryant Mather Int. Conf., J. M. Scanlon, ed., Vol. 1, Detroit, 819–842.
Pigeon, M. (1994). “Frost resistance.A critical look, concrete technology past, present, and future.” Proc., V. Mohan Malhotra Symp., P. K. Mehta, ed., Detroit, 141–158.
Pigeon, M., Marchand, J., and Pleau, R. (1996). “Frost resistant concrete.” Constr. Build. Mater., 10(5), 339–348.
Pinto, R. C. A., and Hover, K. C. (2001). “Frost and scaling resistance of high-strength concrete.” PCA Research and Development Bulletin RD122, Portland Cement Association, Skokie, IL, 74.
Robler, M., and Odler, I. (1985). “Investigation on the relationship between porosity, structure and strength of hydrated portland cement pastes. (1) Effect of porosity.” Cem. Concr. Res., 15(2), 320–330.
Rougeau, P., Maillard, J. L., and Mary-Dippe, C. (1999). “Comparative study on properties of self-compacting and high performance concrete used in precast construction.” Proc., 1st Int. RILEM Symp. on Self-Compacting Concrete (PRO 7), 251–261.
Sakai, E., Kasuga, T., Sugiyama, T., Asaga, K., and Daimon, M. (2006). “Influence of superplasticizers on the hydration of cement and the pore structure of hardened cement.” Cem. Concr. Res., 36(11), 2049–2053.
Schell, H., and Konecny, J. (2003). “Development of an end-results specification for air void parameters of hardened concrete in Ontario’s highway structures.” 82nd Annual Meeting, Transportation Research Board, Washington, DC.
Siebel, E. (1989). “Air-void characteristics and freezing and thawing resistance of superplasticized air-entrained concrete with high workability.” Proc., 3rd CANMET/ACI Int. Conf. on Superplasticizers and Other Chemical Admixtures in Concrete, V. M. Malhotra, ed., American Concrete Institute, Detroit, 297–319.
Stark, D. (1989). “Effect of length of freezing period on durability of concrete.” Research and Development Bulletin, No. RD096.01 T, Portland Cement Association, Skokie, IL, 9.
Szwabowski, J., and Łaźniewska-Piekarczyk, B. (2008a). “The increase of air-content in mix under influence of carboxylate superplasticizers acting.” Cem. Wapno Beton, 4, 205–215.
Szwabowski, J., and Łaźniewska-Piekarczyk, B. (2008b). “The increase of air-content in SCC mixes under the influence of carboxylate superplasticizers.” Cem. Wapno Beton, 4, 205–215.
Szwabowski, J., and Łaźniewska-Piekarczyk, B. (2009). “Air-entrainment problem in self-compacting concrete.” J. Civ. Eng. Manage., 15(2), 137–147.
Taylor, C. P., Kosmatka, S. H., and Voigt, G. F. (2006). “Integrated materials and construction practices for concrete pavement: A state-of-the-practice manual.”, Federal Highway Administration, Washington, DC.
Thomas, D. A., and Wilson, L. (2002). “Admixtures for use in concrete.” CD-ROM­ CD039, Portland Cement Association, Skokie, IL.
Tiong-Huan, W., Daneti, S. B., and Thangayah, T. (2011). “Effect of w/c ratio on air-void system of foamed concrete and their influence on mechanical properties.” Mag. Concr. Res., 63(8), 583–595.
Wang, K., Lomboy, G., and Steffes, R. (2009). “Investigation into freezing-thawing durability of low-permeability concrete with and without air entraining agent.” Final Rep., National Concrete Pavement Technology Center, 50.
Wang, R., and Yang, Z. (2013). “Progress in polymers in concrete.” Adv. Mater. Res., 687, 155–160.
Whiting, D., and Dziedzic, D. (1992). “Effects of conventional and high-range water reducers on concrete properties.” Research and Development Bulletin RD107, Portland Cement Association, Skokie, IL, 28.
Xie, Y., Liu, Y., and Long, G. (2008). “Long-term durability of cement-based materials with very low w/b.” J. Wuhan Univ. Technol. Mater. Sci. Ed., 23(3), 303–308.

Information & Authors

Information

Published In

Go to Journal of Materials in Civil Engineering
Journal of Materials in Civil Engineering
Volume 27Issue 9September 2015

History

Received: Jan 28, 2014
Accepted: Oct 9, 2014
Published online: Nov 12, 2014
Discussion open until: Apr 12, 2015
Published in print: Sep 1, 2015

Permissions

Request permissions for this article.

Authors

Affiliations

Beata Łaźniewska-Piekarczyk [email protected]
Faculty of Civil Engineering, Dept. of Building Materials and Processes Engineering, Silesian Technical Univ., Akademicka 5 St., 44-100, Gliwice, Poland. E-mail: [email protected]

Metrics & Citations

Metrics

Citations

Download citation

If you have the appropriate software installed, you can download article citation data to the citation manager of your choice. Simply select your manager software from the list below and click Download.

Cited by

View Options

Get Access

Access content

Please select your options to get access

Log in/Register Log in via your institution (Shibboleth)
ASCE Members: Please log in to see member pricing

Purchase

Save for later Information on ASCE Library Cards
ASCE Library Cards let you download journal articles, proceedings papers, and available book chapters across the entire ASCE Library platform. ASCE Library Cards remain active for 24 months or until all downloads are used. Note: This content will be debited as one download at time of checkout.

Terms of Use: ASCE Library Cards are for individual, personal use only. Reselling, republishing, or forwarding the materials to libraries or reading rooms is prohibited.
ASCE Library Card (5 downloads)
$105.00
Add to cart
ASCE Library Card (20 downloads)
$280.00
Add to cart
Buy Single Article
$35.00
Add to cart

Get Access

Access content

Please select your options to get access

Log in/Register Log in via your institution (Shibboleth)
ASCE Members: Please log in to see member pricing

Purchase

Save for later Information on ASCE Library Cards
ASCE Library Cards let you download journal articles, proceedings papers, and available book chapters across the entire ASCE Library platform. ASCE Library Cards remain active for 24 months or until all downloads are used. Note: This content will be debited as one download at time of checkout.

Terms of Use: ASCE Library Cards are for individual, personal use only. Reselling, republishing, or forwarding the materials to libraries or reading rooms is prohibited.
ASCE Library Card (5 downloads)
$105.00
Add to cart
ASCE Library Card (20 downloads)
$280.00
Add to cart
Buy Single Article
$35.00
Add to cart

Media

Figures

Other

Tables

Share

Share

Copy the content Link

Share with email

Email a colleague

Share