Natural stone is a common material in historic constructions. Flood events may directly affect surfaces of historic stone buildings. Since ashlars and stone sculptures often carry valuable cultural information, a more detailed knowledge about changes in physical properties due to water saturation is crucial for the assessment of their surface stability in case of flooding. Water saturation of stones leads to loss of mechanical strength and to expansion of volume (hydric dilatation). On the basis of data from literature, a rough scheme of vulnerability is suggested for different kinds of building stones. The majority of igneous and metamorphic rock types with dense crystalline structure are not vulnerable to flooding, whereas some types of pyroclastic rocks (tuffs) as well as clay-bearing sandstones are highly vulnerable. Detailed laboratory investigations on Elbe sandstone demonstrate the influence of petrographic features on material behavior due to water saturation. Results of laboratory tests are in good accordance to on-site observations made after the great summer flood in Dresden, Germany in 2002.
Get full access to this article
View all available purchase options and get full access to this article.
Acknowledgments
The study was supported by the European Commission as part of the research project “Cultural Heritage Protection against Flood” (CHEF) (Contract No. UNSPECIFIED044251) in the Sixth Framework Program on Research and Technology Development. Special thanks are due to Katja Bretschneider for technical assistance.
References
Alfes, C. (1993). Bruchmechanisches Werkstoffverhalten von Sandstein unter Zugbeanspruchung, Vol. 1, Aachener Beiträge zur Bauforschung, Verlag Augustinus Buchhandlung, Aachen (in German).
Barefield, E., and Shakoor, A. (2006). “The effect of degree of saturation on the unconfined compressive strength of selected sandstones.” Proc., IAEG 2006, Conf. of the International Association of Engineering Geologists, Paper No. 606, The Geological Society of London, London, 1–11.
Felix, C., and Queisser, A. (1999). “Lineare Deformation von Sand- und Kalksteinen infolge von Flüssigkeitsaufnahme.”Proc., 5th Int. Coll. Material Science and Restoration, Esslingen, Aedificatio Publishers, Freiburg, 1549–1558.
Götze, J., and Siedel, H. (2007). “A complex investigation of building sandstones from Saxony (Germany).” Mater. Charact., 58, 1082–1094.
Grunert, S. (1978). “Petrochemische Untersuchungen an Kreidesandsteinen aus der Elbezone.” Freiberger Forschungshefte A, 583, 65–104 (in German).
Grunert, S. (1982). “Der Sandstein der Sächsischen Schweiz als Naturressource, seine Eigenschaften, seine Gewinnung und Verwendung in Vergangenheit und Gegenwart.” Habilitation thesis, Dresden Univ. of Technology, Dresden, Germany.
Hawkins, A. B., and McConnell, B. J. (1992). “Sensitivity of sandstone strength and deformability to changes of moisture content.” Q. J. Eng. Geol., 25, 115–130.
Hirschwald, J. (1908). “Die Pruefung der natürlichen Bausteine auf ihre Wetterbeständigkeit.” Z. Prakt. Geologie, 16, 257–264 (in German).
Jimenez Gonzalez, I., and Scherer, G. (2004). “Effect of swelling inhibitors on the swelling and stress relaxation of clay bearing stones.” Environ. Geol., 46, 364–377.
Kleb, B., and Vasarhelyi, B. (2003). “Test result and empirical formulas of rock mechanical parameters of rhyolite tuff samples from Eger’s cellars.” Acta Geologica Hungarica, 46(3), 301–312.
Lin, M. L., Jeng, F. S., Tsai, L. S., and Huang, T. H. (2005). “Wetting-weakening of tertiary sandstones—Microscopic mechanism.” Environ. Geol., 48, 265–275.
Mirwald, P. W. (1997). Physikalische Eigenschaften der Gesteine. Naturwerkstein und Umweltschutz in der Denkmalpflege, Ebner, Ulm, 284–308 (in German).
Morales Demarco, M., Jahns, E., Ruedrich, J., Oyhantcabal, P., and Siegesmund, S. (2007). “The impact of partial water saturation on rock strength: an experimental study on sandstone.” Z. dt. Ges. Geowiss., 158(4), 869–882.
Müller, U., and Riedl, M. (2008). “Volcanic tuff from Ettringen and its interaction with agents used for stone conservation.” Proc., 11th Int. Congress on Deterioration and Conservation of Stone, Vol. 2, Copernicus University Press, Torun, 1001–1009.
Ožbolt, J., Grassegger, G., van der Veken, P., Periskic, G., and Reinhardt, H. -W. (2008). “Experimental and numerical study of hygro-thermo-mechanical properties of Schilfsandstein from Baden-Württemberg.” Environ. Geol., 56(3–4), 535–546 (in German).
Peschel, A. (1974). “Zur Ermittlung und Bewertung von Festigkeitseigenschaften bei Natursteinen.” Z. Angew. Geol., 20(3), 118–128 (in German).
Rodriguez-Navarro, C., Hansen, E., Sebastian, E., and Ginell, W. S. (1997). “The role of clays in the decay of ancient Egyptian limestone sculptures.” Journal of the American Institute for Conservation, 36(2), 151–163.
Schuhmann, H. (1983). “Hygrische und thermische Phänomene bei Naturstein.” Bautenschutz und Bausanierung, 6(2), 54–57.
Siedel, H. (2010). “The city of Dresden in the mirror of its building stones: Utilization of natural stone at façades in the course of time.” Materials, Technologies and Practice in Historic Heritage Structures, M. Bostenaru Dan, R. Prikryl and A. Török, eds., Springer, Dordrecht, 137–156.
Siedel, H., Pfefferkorn, S., von Plehwe-Leisen, E., and Leisen, H. (2009). “Sandstone weathering in tropical climate: Results of low-destructive investigations at the temple of Angkor Wat, Cambodia.” Eng. Geol., in print.
Snethlage, R., and Wendler, E. (1996). “Moisture cycles and sandstone degradation.” Saving our architectural heritage: The conservation of historic stone structures, N. S. Baer and R. Snethlage, eds., John Wiley & Sons, New York. 7–24.
Stiny, J. (1929). Technische Gesteinskunde, 2nd Ed., Springer, Vienna.
Török, A., Galos, M., and Kocsanyi-Kopecsko, K. (2000).“Experimental weathering of rhyolite tuff building stones and the effect of an organic polymer conserving agent.” Stone Decay. Its Causes and Controls. Proc. of Weathering 2000 Conference, B. J. Smith and A. V. Turkington, eds., Donhead, Belfast, 109–127.
Vasarhelyi, B. (2003). “Some observations regarding the strength and deformability of sandstones in dry and saturated conditions.” Bull. Eng. Geol. Environ., 62, 245–249.
Vasarhelyi, B. (2005). “Statistical Analysis of the Influence of Water Content on the Strength of the Miocene Limestone.” Rock Mech. Rock Eng., 38(1), 69–76.
Vasarhelyi, B., and Török, A. (2004). “Influence of the water saturation for the strengths of the Miocene limestone.” Proc., Int. Conf. on Dimension Stone, Prague 2004, R. Přikryl, ed., Balkema Rotterdam, The Netherlands, 107–110.
Weiss, T., Siegesmund, S., Kirchner, D., and Sippel, J. (2004a). “Insolation weathering and hygric dilatation: two competitive factors in stone degradation.” Environ. Geol., 46, 402–413.
Weiss, T., Strohmeyer, D., Kirchner, D., Sippel, J., and Siegesmund, S. (2004b). “Weathering of stones caused by thermal expansion, hygric properties and freeze-thaw cycles.” Proc., 10th Int. Congress on Deterioration and Conservation of Stone, Stockholm, Vol. 1, ICOMOS Sweden, Stockholm, 83–90.
Information & Authors
Information
Published In
Copyright
© 2010 ASCE.
History
Received: Jun 11, 2009
Accepted: Feb 18, 2010
Published online: Sep 15, 2010
Published in print: Oct 2010
Authors
Metrics & Citations
Metrics
Citations
Download citation
If you have the appropriate software installed, you can download article citation data to the citation manager of your choice. Simply select your manager software from the list below and click Download.